STUDY OF STRESS CORROSION CRACKING IN 7079-T651 ALUMINUM

File
Publisher
Florida Atlantic University
Date Issued
1975
Description
This study investigated the stress corrosion cracking
behavior of aluminum alloy 7079 - T651 in two corrosive
environments, sea water and a 3% NaCl-distilled water
solution. Self stressing, double cantilever beam specimens
were employed; and these were stressed at various levels,
exposed in one of the two test environments and crack
extension monitored as a function of time. Equations for
the plane strain stress intensity factor (K1) were compared
and evaluated, with respect to stress intensities calculated
from compliance measurements. Results suggest that stress
intensity is not the only important variable controlling
crack growth rate and a time dependent cracking mechanism
may govern a portion of crack growth.
Note

College of Engineering and Computer Science

Language
Type
Extent
57 p.
Identifier
13730
Additional Information
College of Engineering and Computer Science
Thesis (M.S.E.)--Florida Atlantic University, 1975.
FAU Electronic Theses and Dissertations Collection
Date Backup
1975
Date Text
1975
Date Issued (EDTF)
1975
Extension


FAU
FAU
admin_unit="FAU01", ingest_id="ing1508", creator="staff:fcllz", creation_date="2007-07-19 01:32:10", modified_by="staff:fcllz", modification_date="2011-01-06 13:09:02"

IID
FADT13730
Issuance
monographic
Organizations
Person Preferred Name

FINNEGAN, JOHN EDMUND.
Graduate College
Physical Description

57 p.
application/pdf
Title Plain
STUDY OF STRESS CORROSION CRACKING IN 7079-T651 ALUMINUM
Use and Reproduction
Copyright © is held by the author, with permission granted to Florida Atlantic University to digitize, archive and distribute this item for non-profit research and educational purposes. Any reuse of this item in excess of fair use or other copyright exemptions requires permission of the copyright holder.
http://rightsstatements.org/vocab/InC/1.0/
Origin Information

1975
monographic

Boca Raton, Fla.

Florida Atlantic University
Physical Location
Florida Atlantic University Libraries
Place

Boca Raton, Fla.
Sub Location
Digital Library
Title
STUDY OF STRESS CORROSION CRACKING IN 7079-T651 ALUMINUM
Other Title Info

A
STUDY OF STRESS CORROSION CRACKING IN 7079-T651 ALUMINUM